OverUnity Research

Pulsed / Radiant Energy => Don Smith's Resonant Devices => Topic started by: Peterae on 2009.12.08, 21:40:13

Title: Don Smith's MEG
Post by: Peterae on 2009.12.08, 21:40:13
picture comming
Title: Re: Don Smith's MEG
Post by: Fraser on 2009.12.16, 14:43:03
I have a couple of kgs of metglass ribbon, anyone know of a way to bond this once wound to keep the core solid? At the moment my experiments have yielded noisy cores as the laminations repel eachother when energised, which of course will incur losses. When going above 8kHz I cant hear the vibes but obviously they will still be there only probably not as lossy as the inertia of the material comes more into play and less amplitude in oscillations.
Title: Re: Don Smith's MEG
Post by: Peterae on 2009.12.17, 09:22:54
Hi Fraser

You can but bottles of Quick dry clear Enamel i wonder if soaking in this and then allowing to dry would do the job, i used this on some 1.8 Km wire coils i made for Spherics Tetra build

Peter